Potters & Sculptors - Making Rock from Mud
unsuccessful red river glaze
Tags:
Comment
hi Jeff
I posted it in the technical file under glaze resources and recipes. let me know if you get better results!
Hi Donna,
It wasn't in the Insite data base. Where would I find it? Thanks, Jeff
sure, it's the unsuccessful red river....I would think it's in the data base, but if not I can post it
in reality it is more brown
Hi Donna,
If I may ask, what is the purplish glaze on the left side?
In the discussion forum, in glaze recipes you can search for the c harris temmoko glaze recipe, and at the bottom is some information about the hold and cooling.
I think the hold is at 1850 for an hour and then slow cooling
I was thinking about trying a new firing schedule. Where did you find the one you are planing to use and why are you using it?
thanks, I was disappointed because it was supposed to be orange red, but now I realize I wasn't firing it correctly (with the holds and slow cool)
I'm going to test the c harris temmoko and see if it gives me more of what I was looking for
i like the surface combination, it may not be what you wanted but it looks good from here.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics