Potters & Sculptors - Making Rock from Mud
Slip drizzled and brushed on. Glazed with clear glaze.
Tags:
Comment
Recipe Name: 5-6 Clear
Cone: 6 Color: clearFiring: Oxidation Surface: Glossy
Amount Ingredient
40 Feldspar--Kona F4
30 Gerstley Borate--1999
20 Ball Clay--Old Mine #4
10 Silica
100 Total
Unity Oxide
.3 Na2O
.113 K2O
.01 MgO
.576 CaO
1.000 Total
.768 Al2O3
.558 B2O3
.008 Fe2O3
4.541 SiO2
.015 TiO2
5.9 Ratio
6.9 Exp
Comments: From U Florida midrange glaze base. "Boy, do I have a fabulous clear glaze for you!! I tested about 15 clears last year and only came up with 2 that I would consider using. This glaze is incredibly forgiving - doesn't show drips, overdips, differences in thickness, is glassy clear w/o yellow, and doesn't craze. Can you believe it? I couldn't either, but it's true and I am absolutely thrilled with this glaze. It only has 4 ingredients, too. I use this over slips and underglazes and it's fine. I also use lusters over it with great results. What can I say? This is THE PERFECT clear glaze. Have fun. Laura in Oregon" -----------------------------------Calculations by GlazeMaster™
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics