Comment by Norm Stuart on March 18, 2014 at 10:49pm

Red and orange are very expensive colors if you want them to survive cone 6 or cone 10.  These colors can be achieved at a far lower cost at cone 06 using Ferro Cadmium frits CM-940 for yellow and CM-941 for red.

I have a small container or Coyote Really Red myself.  It's mostly Red Mason Stain, or a competitor product with a smaller percentage of a zircopax-like opacifying product to make the red more intense.  Based on the texture it's likely suspended with a small amount of bentonite rather than a large portion of kaolin like less expensive underglazes.

Mason Dark Red 6088 Stain costs about $37 a pound from Axner.  It's a cadmium-selenium silicate encapsulated in zirconia.  Mason Tangerine 6027 is less costly cadmium-selinate costing under $25 per pound.  Other Mason stains cost less than $15 per pound.

Occasionally you'll find a glaze chemistry which is not compatible with zircon encapsulation resulting in the glaze foaming with either the Mason encapsulated stain or the Coyote Really Red which, tipped me off that RR is mostly encapsulated stain.

http://www.axner.com/mason-stain-6088.aspx

http://www.axner.com/mason-stain-6027.aspx

I both both, along with a selection of less costly colors for our studio.  We mix them with water and gerstley borate, but you can just as easily mix them with bentonite and a small percentage of a Ferro frit to help the stain adhere in the firing.

Comment by Lawrence Weathers on March 18, 2014 at 9:23pm

thanks for the scoop. Maybe we can get Norm Stewart to stir up something like this. That's his favorite entertainment.


Stars
Comment by Brian Dean on March 18, 2014 at 6:22pm

Lawrence, I can't claim credit for this red glaze. It is a commercial Coyote red glaze. Have not found any publicly accessible red glazes like this for Cone 6 oxidation out on the internet that you can just mix up and go. In fact this was probably $8 worth of glaze just on this one bowl. So I use this type of commercial red glaze mostly as an accent glaze but I wanted to make a red bowl so I did it. The brown around the edges is Hanna's Fake Ash over the commercial red glaze.

Comment by Lawrence Weathers on March 18, 2014 at 6:09pm

what is the red glaze used here?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service