Glazes used - Sprayed 'Floating Red' then lightly sprayed with 'Hannah's Fake Ash'.

Views: 117

Albums: Cone 6

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by George Lewter on October 2, 2011 at 5:30pm
Your recipe has the same proportions. It just isn't "normalized" to 100 with the colorants as additions to the 100 g base glaze.  Yours adds to 100 including the red iron oxide.

Stars
Comment by Jan Wallace on October 2, 2011 at 4:43pm

Hi George, No i have not seen the article, but i have a love of all things old and rusty. My new studio has a feature wall (behind the teapot) made from old rusty roofing iron. I would like to see the article though as it sound really interesting. I thought I got the recipe from here, but mine is slightly different. It is as follows;

Gerstley Borate         47.8

Talc                        13.0

Silica                       26.1

does not add up to 100

Add:  Red Iron Oxide  13.0

I have found that this glaze is best thinner, as when it is too thick it is very dark brown all over. Where you see the lighter, yellow/green areas it is thinner.

 

 

Comment by George Lewter on October 2, 2011 at 6:37am

Nice, Jan.

Was this inspired by the oil can teapots in Ceramics Monthly from about six months ago? Is it the Floating Red recipe I posted on this network? I ask because I haven't seen this kind of color development on any of my pots. But then again, I don't think I was spraying glazes when I did my experimentation with Floating Red.

Floating Red Cone: 6 Color: multicolored w iron red
Firing: Oxidation Surface: Glossy

Amount Ingredient
55 Gerstley Borate--1999
15 Talc
30 Silica
100 Total

Additives
15 Iron Oxide--Red

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service