SCM for cool colors under Bill Van Gilders Teal Blue fired to cone 8, SH firing schedule

Views: 153

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Michele Hartung on February 8, 2010 at 6:45pm
Took me a minute, but I am still laughing. "Garagio" it is!

Stars
Comment by Michele Hartung on February 7, 2010 at 10:38am
Joan and Jess,
The yellow iron oxide makes SCM for warm colors. Steven calls this his "SCM for orange." I did not add it for this glaze. I am also not sure why the SCM for cool colors (SCM for white) causes the crystals to appear rusty, but it seems to on this clay body. Thanks again for your feedback, I'm just a lowly garage potter, so you have made me feel like queen for a day!

Stars
Comment by Michele Hartung on February 4, 2010 at 8:30pm
Joan and Jess,
Thanks so much! This is a sprayed layered glaze. The first layer is Steven Hill's Strontium Crystal Magic for white, with Bill Van Gilder's Teal blue over the top. It is oxidation fired to cone 7 with a hold at the top for one hour, bringing it to cone 8. The clay body is Highwater's Loafer's Glory.
Comment by Robert Young on December 6, 2009 at 11:41pm
I love this piece! The shape, the crystal growth in the glaze, AND the coloration!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service