wheel thrown and altered, dark stoneware, soaked in brine and electric fired to cone 5-6

Views: 131

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Joseph Fireborn on December 28, 2015 at 8:04am

So then your firing this cup in a cone 6 electric kiln and getting these results because of the salt brine. That is pretty awesome.


Stars
Comment by Norm Stuart on December 25, 2015 at 9:38pm

Traditional salt firing simply adds dry salt to a hot kiln.  Ron Mello dunks bisque in a salt brine prior to glazing, which I imagine would greatly reduce wear on the kiln.

It's similar, in a way, to what I do with paper clay. On the west coast of America, Laguna Clay sells only Max's Cone 10 paper clay which remains very porous and breakable after a firing to Cone 6.

Rather than pay for a shipment of their Florida-made Sybil's Cone 6 paper clay to California, I dunk bisqued Cone 10 paper clay ware in a solution of 50% sodium carbonate and 50% lithium carbonate and dry prior to glazing. This adds the missing flux the Cone 10 paper clay needs to densify at Cone 6. Sodium leads to a higher COE which is offset somewhat by the lithium.

Comment by Joseph Fireborn on December 25, 2015 at 8:23am

Can you explain what you mean by used soda ash as brine? Are you just soaking this pot in a bag of soda ash wet? It is a very beautiful pot, however you did it, great work.

Comment by Ron Mello on January 20, 2014 at 12:06pm

Hi Norm,

Actually, I used soda ash for the brine. I will have to try the silicate too..


Stars
Comment by Norm Stuart on January 20, 2014 at 11:57am

Have you ever tried sodium carbonate as brine instead of sodium chloride?

Comment by Ron Mello on January 20, 2014 at 4:25am

The color is a glaze that was poured over the dried salt brine soaked stoneware adding depth reduction and color to the clay and glaze.

Comment by Shine Chisholm on January 19, 2014 at 2:24pm

no glaze at all? the color is just the salt?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service