Comment by Jeff Poulter on July 15, 2013 at 8:04pm
Well, I only had red clay shards but they are firing as we speak. I also got some of the Gold but they were out of the Gold Rain. I still have Gold and Gold Rain from before they were reformulated w/o lead. I'll have to dig them out and do a side by side comparison. Jhp
Comment by Norm Stuart on July 14, 2013 at 5:59pm
Comment by Jeff Poulter on July 14, 2013 at 3:43pm

Hi Norm,

      No, but I would like to!  Do you have a recipe?  The best moly crystals I have gotten were with Steve's Brilliant Blue Ink.  It ran alot even at ^4 & it kind of acted like an ash glaze which is not good for moly.  They need a well melted glaze that doesn't move much, that allows the crystals to form.  Since I had to wait so long for the powder, I ordered 2 bottles from Axner.  They should be here tomorrow & I will test as well.  What kind of clay are you using to test on?  I think I can do a porcelain & also porcelain with a manganese slip over.  Also I have some red shards.  Let me know & thanks,  Jeff

Comment by Norm Stuart on July 13, 2013 at 6:18pm

Jeff - Have you ever made a cobalt-saturation glaze?

I received the gold-hued Spectrum Metallic Mirror glaze and it's safety labelled for high levels of cobalt.

You can tell by the wet glaze color there's not a significant amount of manganese dioxide. It looks like just about any glaze which contains a significant amount of iron oxide.

I have it on a test tile waiting for a firing.

Comment by Norm Stuart on July 9, 2013 at 9:40pm

Kathy - These are gold ^5/6 glazes, but you could certainly call them metallic copper.

http://www.kazegamas.com/Golds-C5.htm

The "sculpture glazes" are interesting as well.

http://www.kazegamas.com/Sculpture%20Glazes%205.htm

Comment by Jeff Poulter on July 9, 2013 at 3:16pm

I opted for the 5 lbs cause I want to mix things into it dry.  Also with the 25% discount, it was only $35.63 for the 5 lbs.  It will be interesting to see if I can get it to come out the same as the pre-mixed that you get Norm.  It' a race!!!!

Comment by Norm Stuart on July 9, 2013 at 2:46pm

Axner shipped us a couple of pints of Metallic Mirror today, so I'll have test tiles in a couple of weeks.

Comment by Jeff Poulter on July 9, 2013 at 12:43pm

Well, it looks like I won't be running any tests with it this weekend.  I just got my invoice from Baileys & it looks like delivery will be in 2-3 weeks.  Will keep you posted....   jhp

Comment by Jeff Poulter on July 9, 2013 at 12:18pm

I have ordered 5 lbs., so as soon as we lock down the shipping charge it hopefully will be on it's way.  Baileys has all Spectrum glazes on sale for 25% off through the end of the month, so that makes it doable.  jhp

Comment by Norm Stuart on July 9, 2013 at 11:59am

The best copper recipe I have is the Collin Pearson Bronze ^6 you currently use.

To manganese dioxide add 10% copper oxide for color and 10% china clay to control the viscosity.

I also have this low-fire leaded recipe:

  Bright Bronze ^03 oxidation
69.0%   Ceraflux lead-silicate frit
9.0%   Feldspar G-200 Potash
8.8%   Ferro Frit 3134
7.6%   Manganese Dioxide
3.0%   EPK
1.4%   Nickel Oxide
1.0%   Copper Oxide
0.2%   Titanium Oxide

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014