    I'm glad I'm not the only nut that hoarded the metallics before they were all gone.  I go a bunch of the Spectrum metallics as well, before they were reformulated.  I also bought a bunch of the reds before they were gone, too, as well as Super Spill(I think it had lead in the crystals).  One day I will have to take inventory of what I have.  I would buy it & then just shove it in the basement out of site.  I did actually use some Gold Filigree around Christmas and it wasn't even gelled or settled out or anything.  I was sure surprised since it has been sitting around for so long.  jhp

Comment by Diane De Baun on April 14, 2014 at 11:24pm

Comment by Diane De Baun on April 14, 2014 at 11:23pm

Duncan Sy glazes I mentioned (with clear Black)

Comment by Diane De Baun on April 14, 2014 at 11:21pm

Comment by Norm Stuart on April 14, 2014 at 6:11pm

Smaller kilns tend to cool faster than larger kilns due to less thermal mass.

As a consequence, a computerized controller can be used to create a slow-cool between 1,800 F and 1,500 F to emulate the cooling characteristics of a larger kiln, or even a hard fire brick gas kiln.

Comment by Diane De Baun on April 14, 2014 at 5:44pm

I bought up as much Gold Filigree and and Duncan Sy 553 Antique brass when I heard they were stopping using the leaded ingredient.  Good to find the Aztec Gold, firing also at low temperature.

I also recently got a smaller electric kiln, though much newer than my older larger kiln and there is a difference with certain glazes being fired to the same temperature, like the Copper Adventurine glaze by Mayco and others.

Someone mentioned silver glaze,  I use these 2 by Duncan  Anique Pewter  sy1024 and Heirloom Silver sy 1025.

The pewter is most reliable,  sometimes I have trouble with the Heirloom when fired with certain glazes.

Although they dont recommend it, I usually fire both bisque and glazes together, doesnt bother all glazes and that way I always get a little present with each firing.

Thanks for all the great information!   Happy to find this site.

Comment by Norm Stuart on July 19, 2013 at 9:11pm

As you can see the Spectrum 1116 Metal Mirror is more metallic looking on the porcelain test tile.

Even though the bowl made of WC-401 is a white clay, the glaze is far less metallic turning a shiny pewter on the base of the bowl.

Comment by Jeff Poulter on July 19, 2013 at 2:46pm

I only had the red clay shards & neither the MGM or the Gold liked it.  It didn't like the extra iron or the coarseness of the clay.  It also did not like the moly that I mixed in either.  I think both of these would do better on a porcelain or white stoneware.  Also I think they would look better sprayed.  It is very hard to get an even coat when brushing.  I will have to look & see if I have any ^6 cast ornaments left that I could spray.  I know I have ^04 ones, but they won't work for this.  jhp

Comment by Norm Stuart on July 18, 2013 at 6:38pm

This is our finished product with Spectrum 1116 Metallic Gold Mirror. It actually looks green inside as if it were a copper glaze. I don't understand why it's labelled for Cobalt.

This is Metallic Mirror with Weathered Bronze Green.

Metallic Mirror test tile both sides.

Comment by Jeff Poulter on July 16, 2013 at 9:42am

Still too hot to open this morning, so we'll have wait until tonite.  If it was winter, it would have been cool enough but with summer, the kiln doesn't cool as fast after it shuts off.  jhp

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014