Comment by George Lewter on December 9, 2009 at 7:52pm

The rim is what I was wondering about. You might try a line blend of your rutile glaze at one end and the titanium dioxide version on the other. If you get what you want somewhere in the middle you'll know what the proportion of TiO to rutlie to use.

Stars
Comment by Tracy Shea on December 9, 2009 at 7:05pm
Not sure what you mean by the unglazed area. This is glazed with 2 glazes, both base recipes are in Mastering Cone 6 Glazes by Roy and Hesselberth. The green is clear liner with 4% copper carb, the "iced oatmeal" is glossy base 1 with 13% light rutile. Where they intersect, you get the aqua color. Unfortunately, I have been making this glaze combo for a year until I had to rebuy rutlile. Now, it comes out green- I have lost the blue. The new rutile I bought, even though it was supposed to be light, appears much darker in the bag. I'm wondering if there is increased iron in the rutile and it's messing with my blue. So, I'm going to test this glaze with titanium oxide and see if I can get something in the neighborhood.
Comment by George Lewter on December 9, 2009 at 6:56pm
This is a beautiful variegated green glaze used very effectively with the throwing rings and spiral decoration. Is there more than one glaze? I don't think the unglazed area is a positive design element, based on what I can see of it. That is the only thing that keeps the bowl from being 5 star in my view. I would like to see details about the glaze(s) and application. Or, just send me 5 gallons, please. :-)

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service