6x6 handbuilt dish, creamy matt glaze, with copper, iron, rutile washes applied with brush, sponge, and stick, also licorice and red glaze applied with stick. -going for the impressionistic landscape appearance.

Views: 109

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Jan Wallace on May 16, 2011 at 9:30pm
Thank you Carl. I will certainly have a look at the sites you have suggested. Thanks for the information. I have Mastering Cone 6 on order, but have plently of glaze recipes from this site to experiment with whilst i wait. I have mixed up about 15 so far, but just waiting for my kiln to be fixed :(

Stars
Comment by Carl Ray Crutchfield on May 16, 2011 at 5:01pm
I have not done it yet, so it will be an experiment for me.  I plan to use the schedule from Mastering Cone 6 Glazes, even though I will not be using their glaze recipe.  I have read their book and I am using their colorant combinations with a commercial dry glaze, so I figured why not.  If you have not seen this web site, you might give it a look.  http://www.masteringglazes.com/index.html Their firing schedule is under the frequently asked questions section.  Also, check out the Recent Glaze Experiments section.  And finally, check out http://www.frogpondpottery.com/ which is the web site of John Hesselberth. one of the authors of the book.  Thanks for communicating.  Good success to you as well.  -Carl

Stars
Comment by Jan Wallace on May 16, 2011 at 4:33pm
Great idea. I used to use a white matt glaze some years ago (had a extended break from pottery) and now the frit i used is no longer available in Australia. I used to brush cobalt over the glaze for a lovely effect. I am going to experiment with a few other white matt recipes myself at Cone 6. I have a small electric kiln with a manual controller so going to have to try to perfect the firing and things like slow cooling. I have been reading a few things on this site about how to do that. Any tips from you would be greatly appreciated. Happy potting :)

Stars
Comment by Carl Ray Crutchfield on May 15, 2011 at 7:44pm
thanks for the encouragement Jan, I am working on a load of pieces to glaze with this matt glaze and try to slow cool.  I read up on it and want to give it a try.  Also I want to try some variations on the glaze by adding colorants to the glaze.

Stars
Comment by Jan Wallace on May 15, 2011 at 6:12pm
Very nice Carl. Thanks for sharing the technique you used on this piece. :)

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service