Found it and added it. Thanks Jeff.
The glaze is really not so much a white as a calcium semi-matte, made even more white and opaque from the magnesium in the Dolomite.
Probably like the calcium semi-mattes from "Mastering Cone 6 Glazes", the glaze is fairly stiff so won't interact much with a more fluid glaze layered over it - so an ideal ceramic canvas gesso.
I've found putting down a layer of a ^6 glaze like this can make leaded manganese gold ^06 glazes turn really metallic and lustrous as they provide a platform and seal the low fire glaze off from the clay body.
Hi Norm,
If you do a search on this website for "tabletop", it will pull up Donna's post with the pic at the top. jhp
A photo of Donna's Matte White with just another glaze on the rim would be perfect.
I think attaching those photos is misleading as they were layered with other glazes. There are pics of Donna's White Matt with just another glaze on the rim that would represent the glaze by itself. jhp
So just to clarify, the recipe in the previous post is for Obsidian. I did some hunting & found Donna's White. I call it Donna's White cause it cam e from Donna F, but in reality she just calls it Matt White. It's posted below. I don't know if it is already in the database.
matte white
Cornwall stone 21%
Ferro 3134 22%
Dolomite 21%
Om4 Ball Clay 15%
Flint 20%
_______________________
99%
bentonite 2%
this is a flat matte white glaze, smooth surface,my experience has been firing it from cone 5-6 1/2 with good results
for colors add
.50% periwinkle blue
4% rutile for a semi matte white, that breaks over dark clay nicely
4% CuCO3 for a copper matte
3% RIO, 1.75% CuCO3, .375% magansese dioxide, .50% rutile for a mustardly brown green
I just checked Eric Preece's blog and what I found was 75 % Alberta, 25 % 3134 & 5 % Cobalt Oxide jhp
I thought it was already there. I know its on the site cause that's where I got it from. It came from Donna Ferrera. I thought she had put it in there. Frogskin is in there as it came from Kathy Ransom. Obsidian came from a guy that used to be on here but I don't think he has been for quite awhile. I think Obsidian is 80 % Albany or a reasonable facsimile thereof, 20 % GB and 5 % Cobalt Oxide.... I'll have to check for sure. jhp
Very nice Jeff. Do us all a favor and add the recipe for "Donna's White" to the Insight-Live glaze database.
Or email me the recipe and I'll add the recipe.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics