Comment by Louis Ford on October 2, 2012 at 6:16am

Here is a good article regarding the cracked ice glaze

http://ceramicartsdaily.org/ceramic-glaze-recipes/mid-range-glaze-r...


Stars
Comment by Catherine Rehbein on October 1, 2012 at 3:17pm

Great to hear from you Louis! The Internal glaze is Soft White an old standby I have used and loved for 15 years! The crackle glazes I do use on the exteriors. The glass is used in decorative pieces and I have never had a problem with breakage. I have purchased a dry mix snowflake glaze

cone 6 ....have not used it yet??? I'll let you know how it goes. Cathe


Stars
Comment by Louis Ford on October 1, 2012 at 10:46am

Hi Catherine...long time.  Couple questions:  Have you tried the fractile glazes?...i've been wanting to make a 'cracked ice glaze' , but haven't gotten around to it.  When putting the glass in you work, have you had a piece break (due to differances in expansion/contraction)?  How durable is the work with glass?  Any chipping orr of the glass?  I assume pieces with glass are decorative only.  In regards to the crazing glazes you use on the cups...I'm guessing the white is interior for safety/durability and the crackle is external? 

Hope this finds you well....Louis


Stars
Comment by Denise Rainville on September 26, 2012 at 9:56am

Thanks, you get it right with your colours.  Lets hope my choice of glaze will work as well as yours.


Stars
Comment by Catherine Rehbein on September 25, 2012 at 5:09pm

Denise , I do not mix my own glazes....I used  Laguna Catalina crackle, Soft white, in the above piece. I even use broken window glass if I feel the glazes will not mesh.. I pour them quite thick, sometimes they do not flow .cant remember if it was done here??? I often times throw stained glass pieces in left over from windows I have done in the past.   I am anxious to try the new celedons from  e.coleman...these look like they would be a great addition ! Good luck!


Stars
Comment by Denise Rainville on September 25, 2012 at 4:23pm

Catherine, I am always in awe of your work.  In the above, I particularly like the glaze on the inside of the tray.  Could you tell me what it is?  I want to simulate water in my current work (both blue & green) and  I need it to be transparent as there is texture on my pieces.  I would greatly appreciate the recipe if possible.  Denise

Comment by Christopher Cisper on May 31, 2012 at 8:04am

Amazing.... as always


Stars
Comment by rose maguire on May 30, 2012 at 8:31pm

Well done...Youve given me the push? inspiration to get off this darn computer and get out to that studio...Must stay focused...Must stay focused...Must stay focused...


Stars
Comment by Catherine Rehbein on May 30, 2012 at 8:22pm

I am ...but you know how it goes, you always find something you might do different the next time. That's what keeps us motivated....that ideal form! This was the first time I played around with slapping down thick plates....had fun and took out some frustration :)


Stars
Comment by Catherine Rehbein on May 30, 2012 at 8:19pm

Thanks Rose! Had fun making them. Just took them out..didn't even try them yet. Photographed them for SFPN ??? We'll see if they make it?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service