Adventuring into using multiple glazes for a more interesting surface.

Views: 161

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Sharon Canfield on February 14, 2017 at 6:41am

I should add that I only put Waterfall Brown on the top third of the piece so that gives you an idea of how much it ran at Cone 6 too.


Stars
Comment by Sharon Canfield on February 14, 2017 at 6:39am

It didn't run off but did form a roll of glaze at the bottom.  I think it was pure luck that it didn't run off.  We did have the piece stilted. Waterfall brown is a runny glaze to start with and if applied to thick definitely will get your kiln shelf.

Comment by Hilltop Pottery on February 14, 2017 at 6:18am

Did this pool heavily at the bottom?  It looks like it pooled on the kiln shelf.  The outcome is lovely though


Stars
Comment by Sharon Canfield on December 10, 2012 at 8:15pm

I make our own glazes so they are not something you would be able to purchase.  The key to the results however, was using a matte glaze first, a clear shiny transparent glaze on top of that and Mastering Cone 6 Glazes Waterfall Brown tweaked for our stoneware clay and firing schedule.  


Stars
Comment by Kabe Burleson on December 10, 2012 at 7:05pm

Looks like you ended up with a very pleasant Adventure. Very nice.

Comment by Leigh Whitaker on December 10, 2012 at 6:46pm
Very nice!
Comment by Darlene Shemanski on December 10, 2012 at 6:26pm

Sharon, you goal was accomplished... nice going! It is beautiful. Would you share which glazes you used.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service