Comment by Cyndy Littleton on April 14, 2015 at 11:35am

Love the recipe! It's gonna have to be a glass of wine instead of a brew though.


Stars
Comment by Brian Dean on April 14, 2015 at 11:30am

Cyndy:

I use this Terra Sig Recipe and process. Brush it on. Many coats then polish with soft cloth before bisquing.

http://www.futurerelicsgallery.com/blog/charlies-home-brew-terra-sig

Brian Dean

Comment by Cyndy Littleton on April 14, 2015 at 11:16am

I have never used terra sig. Do you brush it on, then wipe? I usually just grab a polishing stone and start rubbing before bisque firing.


Stars
Comment by Brian Dean on April 14, 2015 at 11:06am

Cyndy, yes I've found the same thing. So I line the bottom of the container with cut sheets of newspaper then cut and put multiple sheets around the circumference of the pot. Last, I put several damp sheets on the inside top cover which prevents old ash from falling into pot. Then after putting pot into reduction container and putting lid on, I cover the container with an old damp towel to minimize smoke escaping and freaking out the neighbors.

Also, all my raku these days I terra sig before bisque firing to create a shiny surface. Then apply my tape decorations, brush glaze, then remove tape then fire. I like the shiny black surface that terra sig'ing the pots creates.

Comment by Cyndy Littleton on April 14, 2015 at 10:58am

Great! I've tried straw and another time shavings. Both will leave marks in the glaze. Some people call it character. I prefer not to have marks. Will try newspaper next time.


Stars
Comment by Brian Dean on April 14, 2015 at 10:37am

Cyndy, just using newspaper!

Comment by Cyndy Littleton on April 14, 2015 at 10:30am

What are you using as your combustibles during your reduction?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service