Been a while since I posted anything. Took a break from burnout for about 7 months.

This is a result of a lot of testing of random surface designs and glaze mixtures. This is the best result I have gotten so far. Sharing for thoughts.

Views: 107

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Erik Evans on May 9, 2017 at 6:08pm

Now, ain't that the best?  Nice work.  I know that feeling.  Excited for you.  The freshness of a pot at this stage is so seductive.  Such a shame we can't capture that indefinitely.  Good luck!

Comment by Joseph Fireborn on May 9, 2017 at 5:39pm

Yea no problem. Thanks for commenting. I haven't done much work with this lately, been making different things and testing a lot. I have been wedging in course grog and sand in my new work. I threw some pots today without sand and grog and I felt empty. I doubt I will continue throwing without sand/grog in the future. Just so much more satisfying for what I want in my work. 

Here is the best greenware pot I have made yet: http://josephfireborn.com/wp-content/uploads/2017/05/yunomi.jpg


Stars
Comment by Erik Evans on May 9, 2017 at 5:36pm

Awesome.  Thanks.  

Comment by Joseph Fireborn on May 5, 2017 at 4:37pm

Oh, and this was just a bunch of glazes layered in a unique way along with a lot of finger swipes, cuts in the surface etc. No rough particles here. But I am currently testing course grog and sand in my porcelain work. Really enjoying the texture.

Comment by Joseph Fireborn on May 5, 2017 at 4:36pm

Sure! Thanks.

Here is a link to a larger photo of it. https://i.redd.it/ijr0wizxicsy.jpg

I have put this on the back burner for a while. Working with black porcelain at the moment. Trying a lot of new things.


Stars
Comment by Erik Evans on May 5, 2017 at 4:33pm

Impressive results here, sir.  Is a rough mix or coarse particle size part of your bag of tricks?  And would you mind posting slightly larger photos?  Pots like these beg to be examined more closely.  Nice to see you back.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service