Gardside base with copper added

Views: 131

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Tess van Dijk on May 14, 2011 at 4:36pm
Thanks Kathy. I have had some crazing on certain tiles with certain colorants. But nothing that I really cant fix. I agree it seems to be fit thats the only issue. I love his base. It really has lots of possibilities.

Stars
Comment by Kathy Ransom on May 14, 2011 at 8:24am
I really like Gartside base too and have been trying it with different colorants.  I emailed him and he replied and said some people found it crazed but I've not had that happen and think it may be an issue of fit.  I will put up some photos of my results soon!

Stars
Comment by Tess van Dijk on April 22, 2011 at 5:27pm
This is the Brian Gardside base found in the work of Alisa Clausen. I added 3% copper to this base. I haven't had time to test if for running off the tile. It is a wonderful base that has a lot of possibilities. I plan on testing this in the future. It may very well be a nice cone 6 celadon. If you look up Alisa and her work you will find his bases, this one is a shiny base. Clay thread art is where I started my search for bases. I only take the base and then add my own colors as I choose.
Comment by Zoophagous on April 22, 2011 at 1:03pm
ooo love this one. Care to share the recipe?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service