Colours do not always turn out how i expect.

Views: 135

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Marina Reijsmeijer (Kleierij) on October 28, 2015 at 4:05am

I added the MDblack to Insight. It is indeed a glaze with no cobalt, but when i tested it (a long time ago) it did turn out black in ^6ox. I will  not pursue this glaze further because Ron Roy's licorice works well for me. 

I found the persian blue glaze in a facebook discussion and fell in love with it. I had already tested my own base glaze that contains 5% barium with CupperCarbonate and it always turns green, but I decided to try the persian blue anyway. Actually the test with 1% cuppercarbonate is better.  You are probably right that I should add more Ba.

Both recipes are cone 6 ox. facebook Heath 


Stars
Comment by Norm Stuart on October 27, 2015 at 10:15am

It's has really nice colors for a mistake.  You'll have to add the MD Black to Insight-Live, but from the color it looks like a black glaze without the addition of cobalt. This sort of "black glaze" turns black in a Reduction firing without Cobalt due to the Fe2O3 red iron oxide becoming Fe3O4 Black Iron Oxide. But in an oxidation firing, this type of black comes out brown.

The color mechanism of the Persian Blue recipe appears to be copper interacting with barium or strontium.

Strontium carbonate creates much lighter blues than barium carbonate. 

The Strontium/Barium + Copper glazes I use have at least 30% Strontium Carbonate or Barium Carbonate, compared with 6.5% in Persian Blue. Dark Blue where thick and light blue where thin.

Based on Tracy Wilson's comments in Barium Blue Matte, these glazes may develop more dark blue color at a Cone 9 Reduction.

Is it possible both of these recipes are meant for a reduction firing which should be coded RX?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service