Cress customized face-plate for the Bartlett V6-CF Controller with Type-K thermocouple

Going back to Bartlett to get a software update and fitted with a Type-S thermocouple.

Views: 205

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on November 3, 2013 at 10:06pm

Bartlett returned the motherboard board with Type-S thermocouple, but without Type-S lead wire.

We used longer screws on the mounting block, placing the thermocouple through a 1" thick kiln post, like those shown below between the exterior kiln wall and the mounting block, to achieve the correct 3/4 inch to 1" exposure inside the kiln. The standard Type-S thermocouple is longer than the Type-K.

http://a248.e.akamai.net/origin-cdn.volusion.com/qz29d.hncd6/v/vspfiles/photos/KLN-800-1.jpg?1369823725

Lead wire for Type-S apparently has to be shielded as Type-S uses only 0-18.6 milliVolt, while Type-K uses 0-54.8 milliVolt which is less sensitive to EMF noise. 2,232 F (^6) is 12.22 mV with a Type-S vs 49.65 mV with Type-K.

http://us.flukecal.com/Thermocouple-Temperature-Calculator

EMF noise from the power relays has led to ERR-1 on ^6 firings using Type-K lead wire.

Correct Type-S lead wire is $4 a foot from L&L Kilns.

Thermocouple Lead Wire - Type-S

http://hotkilns.com/thermocouple-lead-wire-type-s


Stars
Comment by Norm Stuart on August 26, 2013 at 4:59pm

All of the control features not on the faceplate are activated by rotating through a menu with the

"F or C Select" button.

CHG°- Change between °F and °C
ErCd – Turn Error Codes on or off
tCoS – Set Thermocouple offset
dELA – Set Delay start
bd t – Displays Board temperature
rSEt – Resets board to default settings
PrHt – Set Preheat segment
Id – set controller ID number
16-S – Combines user 5 and user 6 programs to achieve a 16 segment program.
CnoS – Set cone offset.

The holds, delays, pre-heats, etc are all entered in the form of 00:00 Hours:Minutes.

We've reprogrammed User 6 ramp with our slow-cool at 50F per hour between 1,800 and 1,500 F.

To activate the slow-cool we have to "F or C" to 16-S and hit enter, to decouple User 5 and 6 from their normal 16 step program capability, then hit the Ramp button and enter.

User 1 is a glass slumping program

User 2 is a glass tack fuse program
User 3 is a glass full fuse program
User 4 is a glass bead-annealing program
User 5 is a lost-wax burnout program
User 6 is a slow cooling cycle that can be added to the end of a cone 6

Choosing the rSEt button, and typing in 443, gives you NOTC - a hidden menu which displays the total number of firings, reconfigures the kiln for an Type-S Thermocouple, also this also requires moving a jumper on the CPU board, makes other configuration changes and recalls prior Error Codes.

I used the CnoS Cone Offset button once to re-program our cone 5 to a cone 5.5, but we've since reset it.

Firing the Cress is not more complicated than microwaving a frozen entree.


Stars
Comment by Jeff Poulter on August 26, 2013 at 2:08pm

5 speeds, no waiting!  On Skutt you get Fast, Medium & Slow & on L&L you get Fast & Slow Glaze & Fast & Slow Bisque & on Orton you get their standard programs & you either speed them up or slow them down by percentages.  Never seen a Cress close up & personal before!  jhp


Stars
Comment by Norm Stuart on August 26, 2013 at 2:05pm

This is the faceplate on an unmodified Bartlett V6-CF.

V6CF Controller


Stars
Comment by Norm Stuart on August 26, 2013 at 2:02pm

This is a Bartlett V6-CF controller with a faceplate customized for the Cress E-23 kiln.

It's on its way back to Bartlett for a software update and to be fitted with a Type-S thermocouple. Each of 6 User programs will have 16 steps rather than the current 8, and User 5 and 6 can be combined into a single 32 step program.

But I have found the "Cone Fire" option is very reliable. We'll see if we notice a difference with the Type-S platinum/platinum-rhodium thermocouple.

It's just like using a microwave oven - I'd never go back to a kiln-sitter.

Were it not for the software update, the change from Type-K to Type-S thermocouple could be done simply by moving a jumper on the CPU board from one pin to both.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service