Using Witness Cones to verify the Cone measurement of our new controller without a slow-cool I added tiles of some popular glazes.

Clearly, Orange Street would not be a Studio favorite without our 6 hour slow-cool.

The look of a "Cone 10" glaze is almost exclusively a result of slow-cooling caused by the heavy firebrick.

In an electric kiln with fast cooling foam brick you have to add heat as it cools to achieve the same result.

Views: 107

Albums: Glaze

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Norm Stuart on September 29, 2017 at 9:07pm

Very nice. A 50 F per hour slow-cool provides the same look as a hard fire brick kiln which naturally cools that slowly.

Comment by Joseph Fireborn on September 29, 2017 at 7:44pm

Ran the schedule. Everything came out very nice. Going to keep using it for a while. Mixing up some orange street this weekend and firing it. Thanks for all the posting you do on these forums Norm. 

This was the result of your schedule: https://www.instagram.com/p/BZpLvzblSjT/

Comment by Joseph Fireborn on September 28, 2017 at 2:41pm

I am only firing one iron glaze this go around, but I am sure the others will show up interesting as well. 

Comment by Norm Stuart on September 28, 2017 at 2:15pm

Most iron glazes change appearance greatly with the slow-cooling speed.

There were some popular (non-iron) translucent glazes which became too opaque and crystallized with a slow-cool.

So some, like Tang Lime, I converted to low-fire bisque-temperature glazes;

Others became new interesting and different Cone 6 glazes with the addition of 20% of a very fluid frit added.

Each of five frits I used to add 20% to the original recipe made a completely different glaze - it's kind of fun - Ferro Frits 5301, 3269, 3134, 3110, 3124.

You can also try the higher magnesium 3195 or high magnesium 3249, but these tend to make semi-mattes out of the glazes which over-crystallize in a slow-cool.

There's always at least one winner.

Comment by Joseph Fireborn on September 28, 2017 at 1:08pm

Going to run your schedule tonight to see how it looks on my current line of work. Trying to lower my total schedule from 16-17 hours down to 14-15. I will post some results under pictures when I take it out. Hopefully it looks as good as this! hahah. Although no orange street in there this time. But I am going to mix up some of that glaze if I keep running this schedule.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by