Hannah's Fake Ash blue above Variegated Slate Blue over Nutmeg

Views: 313

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by George Lewter on November 5, 2011 at 10:35pm
I use C Harris temoku as a liner most of the time because of its reliability, and because it has no toxic colorants.  A little iron leaching isn't even an issue.
Comment by Margie Cleveland on November 5, 2011 at 7:41pm
Is Nutmeg your liner glaze?
Comment by Jan Wallace on November 3, 2011 at 3:44am

Thanks George. I will give it another try. Although, I must say that the nutmeg recipe I used (the revised version of the recipe) was a little dry, possibly underfired after firing, so this could be a factor. Although there are so many variables of course that could have played a part.

Think I found these recipes on the Alisa Clausens website, if not this one?

Recipe Name: Nutmeg RR Revision.

Cone: 6 Color:
Firing: Surface: Glossy

Amount Ingredient
22.5 Dolomite
19.5 Feldspar--G-200 ( I substituted for Potash Feldspar)
10 Spodumene--Foote
7 Frit--Ferro 3134
22.5 Ball Clay--Old Mine #4
18.5 Silica

100 Total

Additives
1.1 Iron Oxide--Red
3.2 Ochre--Yellow
4.9 Tin Oxide

I have mixed up another (below) and trying this one on test rings in a kiln load tomorrow, so I will let you know.

Recipe Name: Nutmeg

Cone: 6 Color: Tan - light brown
Firing: Oxidation Surface: Semiglossy
Amount Ingredient
23.3 Dolomite
23.3 Spodumene
6.8 Frit--Ferro 3134
23.3 Silica
23.3 Ball Clay--Old Mine #4
100 Total

Additives
1.1 Iron Oxide--Red
4.9 Tin Oxide
3.2 Yellow Ochre
1.9 Bentonite

Comments: Richard Busch Ceramics Monthly 2/2003
Author mixes this glaze 2/3 with 1/3 Busch white satin matte
By itself a warm tan breaking brown over iron bearing clay body

 

Comment by George Lewter on November 3, 2011 at 3:18am

I believe I sprayed nutmeg first only on the bottom half, then the Variegated Slate Blue again only on the bottom half.  The Hannah's Fake Ash Blue was sprayed by itself at the top and lapped slightly over the other glazes in the middle. The clay is Laguna B-Mix 5 white stoneware which shows through in the thinning between the rivulets.

Comment by Jan Wallace on November 2, 2011 at 10:38pm

Loving this glaze combination. Must try this again myself. I had no luck with this combo in my last lot of tests.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service