Outside - Nutmeg base. Layered on JJF at top and Watercolor green in middle
Inside CHT
On Laguna B-Mix 5 clay
Tags:
Albums: Single Fire Success Story
Comment
C Harris Temoku poured inside
Nutmeg sprayed over entire outside (medium coat)
Band of Jens Juicy Fruit sprayed on outside top 1/3 (thin coat)
Band of Water Color Green sprayed overlapping the JJF and down onto the Nutmeg. (thin coat)
Be careful with Water Color Green as it is quite runny.
Thank you, Robbie.
CHT = C. Harris Temoku
JJF = Jen's Juicy Fruit
The spectral effects on the outside at the very top seem to involve the small amount of CHT that is diffusing from the rim. You can see it on several of the cups from this series. Not sure about the blue/purple, but Steven Hill has gotten effects similar (and better) with the reactions of JJF and Strontium Crystal Magic and Spotted Black. I have yet to pull any more saturated yellows, oranges, reds, or purples with any these combos, just hints that the colors are there waiting to be released.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics