BMix-5 white clay - 5X5 - Nautilus is Sapphire Blue, 12% Iron, Black, Really Red glazes over White Liner - Border is Copper Wash over White Liner

Views: 92

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Nadine Mercader on September 23, 2012 at 11:22am

Thanks for the info Carl!  I also build my own glazes,  don't use any commercial.  I love the effect your wash gives.  I love texture.  I am really into slab work recently and that allows for great texture.  I also love carving leather hard clay.  

I have been many times to Mobile,  a great place to live!


Stars
Comment by Carl Ray Crutchfield on September 23, 2012 at 11:08am

Thanks Nadine.  I build all my glazes, or at least the vast majority, by adding oxides and carbonates to a clear commercial glaze that I buy in dry form.  The piece here is covered with a coat of what I call my white liner - clear glaze plus 12% zircopax.  The clay is BMix-5 white clay but I like to use the white liner as it mask any irregularities in the surface, which a clear glaze does not.  The wash on the rims is a mixture of clear glaze and copper carbonate in a 5 to 3 ratio and diluted to a thin wash with water.  It has been brushed on with a hake brush over the white liner about 2-3 passes with the wash.  Love your use of texture by the way, I really like to use texture in clay also.  take care, carl


Stars
Comment by Nadine Mercader on September 23, 2012 at 10:50am

What a gorgeous piece!  Please tell me about the copper wash etc...


Stars
Comment by Carl Ray Crutchfield on May 26, 2012 at 7:21pm

Thanks, Jan appreciate the support.


Stars
Comment by Jan Wallace on May 26, 2012 at 3:48pm

Great results Carl. Particularly like this one. 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service