Cone 6 electric. Porcelain. Lorio ash (modified), seiji nuka (modified). Matching salt and pepper shakers.

Views: 165

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Zoophagous on March 30, 2010 at 7:47pm
Thanks! I did line tests to drop the glazes from cone 10 to cone 6. I don't have the recipes handy but I recall posting the lorio ash one in the recipe section of this site. I got the original from John Britt's book.
Comment by Zoophagous on December 19, 2009 at 10:15am
Hey George,

Yes, the inner wall is just an open cone. Turn the shaker upside down and pour in salt (or pepper) then just turn right side up again. Similar to the cadogan teapot. Sounds strange but works =)
Comment by George Lewter on December 19, 2009 at 7:08am
On your http://ultramegaceramics.blogspot.com/ blog you detailed throwing salt and pepper shakers. I'm a little confused about the technique. Is the inner walled cone so that the shakers don't require a cork or other seal or just so the seal is recessed?
Comment by George Lewter on December 18, 2009 at 7:57pm
That pepper shaker really does it for me, Eric. The plate is pretty sweet, too.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service