4x4x5 B Mix 5 cone 6 clay. creamy matt over copper wash. I plan to build a handle from copper and oxidize it and attach through two holes in the lid. I really like this piece, but I has stress cracks at the lid on two corners. I will try again.

Views: 133

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Carl Ray Crutchfield on April 15, 2011 at 5:53am
I posted a second photo this AM.  It may be helpful to know also that the copper wash I use was made from equal parts by volume of copper carb and a clear gloss glaze.  Also, the copper wash was applied quite heavily and wiped down with a damp rag - wiped less so in the texture areas than in the non-textured.  From my test tile, I knew the copper would go black in the texture if left fairly thick, and that was an effect I wanted on the box.  Both the clear glaze and the creamy matt are commercial glazes that I buy in dry bulk from Coyote.

Stars
Comment by susan claysmith on April 14, 2011 at 9:02pm
I am seeing the colour as a pale turquoise; it will be interesting to see another shot of this considering that you say that the colour is a bit less intense than this photo.  I am definity going to run a test tile and try for this effect - I imagine that the overall effect could be quite different depending on the composition of the matt glaze.   Again, a very nice piece.  Susan

Stars
Comment by Carl Ray Crutchfield on April 14, 2011 at 7:13am
Thanks, Tracy.  It is all coming from the copper carbonate.  the browns and blacks are a heavier application of the copper.  also, the greens are not a bright as they appear in the photo, they are softer with just a few bright spots along edges.  I may try another photo later.

Stars
Comment by Carl Ray Crutchfield on April 12, 2011 at 5:02am
Susan, your my first commenter, ever....... thanks for the encouragement.  The Creamy Matt is a premixed glaze from Coyote.  I don't believe it has any colorants in it, when fired plain, it is white.  It has a very soft touch, and really reacts well to the copper wash.  I also tested it with an iron wash and a rutile wash, but it did not work so well with them.  Again, thanks for the interest.  -carl

Stars
Comment by susan claysmith on April 11, 2011 at 8:45pm
Hi Carl - I really love the overall look of this piece and the glazing effect is excellent.  What colourants are in the creamy matt glaze?  Susan

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service