Comment by Jan Wallace on May 5, 2011 at 5:33pm
Thanks Miri. I appreciate you sharing your knowledge. I am very excited to try these glazes myself. My kiln is broken at the moment and hoping to have it fixed within the next week. I have mixed all my glazes and made a heap of test rings, so i am desperate to start and see what happens. I have a manual kiln, so a little nervous that i won't get the same results as those with controllers who can set a recommended firing schedule...
Comment by Miri Hardy on May 5, 2011 at 4:04pm

Thanks for the compliments.  I always glaze by dipping.  This was dipped half in the black (once), then half (overlapping over the black) in the red (once).  

 


Stars
Comment by Jan Wallace on May 5, 2011 at 3:18pm
Hi Miri. I can see that this is dipped on one side, but can i ask please, do you generally always dip your glazes or do you also spray? Also, how many times would you dip the piece to achieve this result. Thanks. Very Nice!
Comment by Miri Hardy on May 4, 2011 at 8:59am
No problems! :-)  I do sooooo much experimentation with my glazes.  Glaze thickness is but one variable but BOY is it important.

Stars
Comment by Michele Hartung on May 4, 2011 at 7:37am
Wow, you really nailed it.  It gives me hope for this glaze.  Thanks, Miri.
Comment by Miri Hardy on May 3, 2011 at 2:51pm
The left side of the bowl is the raspberry on its own.  The overlap with LB is only in the middle.  Perhaps your glaze is thinner than my application?

Stars
Comment by Michele Hartung on May 3, 2011 at 2:37pm
Do you think it's because the raspberry is over the black that it's such a pretty red?  Are you getting this color on the B-mix alone?
Comment by Miri Hardy on May 3, 2011 at 2:00pm
Thanks Michele.  This is on B-Mix.

Stars
Comment by Michele Hartung on May 3, 2011 at 1:42pm
Very nice clean look!  What color clay body are you using?  My raspberry looks pink on most everything I have tried it on.
Comment by Miri Hardy on February 10, 2010 at 8:22am
The red is Raspberry, also in the book.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service