Potters & Sculptors - Making Rock from Mud
10" Vase w/black on the inside and persimmon over an iron red on the outside.
Tags:
Comment
George, I just saw this morning the recipes for discussion page with 'persimmon' on it. I had mentioned awhile back that my glaze wasn't public because the persimmon isn't from the Sankey Glaze Database. Having said that, many glazes can be made successfully a number of different ways -- so perhaps the recipe posted there works fantastic, it just isn't the recipe I use.
Simply beautiful. A couple of Persimmon variations are in the Recipes for Testing Discussion. No one has verified if they are the same Persimmon that Steven Showalter or other members are using.
@Michele, the persimmon glaze has some lithium in it and when it is applied over both the iron red and also the black it has a similar effect. I'm a big proponent of massive testing, and sometimes with all that testing you get lucky, and if you do enough testing you start to see trends and things become much easier to predict.
All my work that I put on this website is at cone 6, but I also sometimes do cone 10 reduction and I also have a wood-burning kiln I fire too. I just meant that at cone 6 you have to do a bit more work on your glazes whereas cone 10 things you can rely more on the flame.
Iron reds do take quite a bit of work/testing at cone 6, whereas at cone 10 I don't find a whole lot of trouble with them. Its nice when you have one that works!
CHT (C Harris Temoku) is probably the best iron red I have ever used. Very repeatable.
Persimmon is not a 'public' glaze. When used over this particular version of iron red it produces a copper iridescence. When used by itself it is orange with some iridescence too. What is CHT?
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics