Also, my extruder is not THAT large... the hollow dies are about 5" in diameter.

Comment by Susan Amann on March 2, 2012 at 7:49pm

Terra Sig:  

Water     6 cups

OM4       4-1/2 cups

sodium silicate    1-1/2 tsp

Mix liquids then add clay.  Mix and let stand 36 hours.  Three layers will form.  Siphon off and discard top layer, collect middle layer, discard bottom layer.

For colors, for 1 cup terra sig base, add:

Green: 2 tsp Crome oxide

Warm Brown: 1 TBL RIO

Dk Grey Black:  4 tsp black mason stain


Stars
Comment by Louis Ford on March 2, 2012 at 7:47pm

do you make those beautiful handles?

 


Stars
Comment by Louis Ford on March 2, 2012 at 7:42pm

yes....i was just looking for one on line......wow, you have a large extruder!  I have a friend that goes to a plant where they extrude large terrcotta pipes for a city.....she goes maybe one time a year.......makes beautiful, large garden sculptures (barbara kobylinska) check out her work

Comment by Susan Amann on March 2, 2012 at 6:44pm

Funny Louis... this started out as a beginner, extruded pot project, so I wasn't initially planning on doing sgraffitto.  I coated the clay with black terra sig and scraped away the black.  It has a clear glaze over it.  Haven't forgotten about getting you the recipe for the naked raku slip resist.  Do you need the black terra sig recipe?


Stars
Comment by Louis Ford on March 2, 2012 at 5:58pm

Love the look of this.....Are you using a black slip? (recipe) or a commercial velvet ? .   Do you paint the whole thing black and then scrape/carve?  A white clay body would really make this pop.

Comment by Susan Amann on February 29, 2012 at 5:54am

Thanks so much Joan... I'll have to put up another photo of the back of this... kind of a "country bird/city bird" piece.


Stars
Comment by Joan Scott on February 28, 2012 at 8:11pm

Wonderful graphics and almost looks like it is a woven birch bark basket

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service