Comment by Bonnie Sherer on February 11, 2014 at 4:12pm

Joe - Thanks for the follow-up.  I just unfamiliar with this website.  Yesterday I signed  in just to ask questions.After sending the message I thought I remembered being interested in it because it was Cone 6 related. Well good , I can try this combination.  I think they are very nice.  I saw glaze effects like this in reduction with SCM.  That buttery warm collection of colors, great bowls. Bonnie


Stars
Comment by Joe Shaw on February 11, 2014 at 11:20am
I sprayed the SCM on the interiors and then dipped the bowl. I fire cone 6 electric with a slow cool-down.
Comment by Bonnie Sherer on February 11, 2014 at 7:44am

Hey there-  You were my first blog and you answered! Thanks.  So it's the warm SCM- maybe brushed and a complete dip with RRed.  Cone 10 w/ reduction?  Did I get it?  :)  Bonnie


Stars
Comment by Joe Shaw on February 10, 2014 at 2:58pm
Yes I do. I'm always glad to share information

SCM on the interiors and then dipped in Randy's red to a six count.
Comment by Bonnie Sherer on February 10, 2014 at 10:38am

Joe Shaw hello-  I may just be missing any comment you have posted. Do you comment on the glaze work associated with these bowls?  Thanks  Bonnie

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service