Comment by Joe Shaw on October 23, 2012 at 9:28am

I sprayed the SCM Warm on the interiors of the bowls and then dipped the bowls in Randy's Red that I had replaced the RIO with Spanish RIO. This meant that I didn't have to use glaze catchers.

I had some problem with glazes (not all) pin-holing so I slowed the cool-down from 2180-2140 from 100 to 40 degrees. After that I let it cool to 1700 at 300 degrees an hour, hold for 60 min., cool to 1600 degrees at 50 degrees an hour then off.

Since slow cooling tends to help produce matte surfaces and my technique usually produces mattes the main conclusion I can come to is that the dipping produced a thicker layer of glaze for the melt.

The glossy surface should be more food friendly. We're pleased and our customers seem delighted. The color response seems far more interesting than I was getting before. I try to enhance that by swirling slip around the interior for glaze breaks.

Comment by George Lewter on October 22, 2012 at 9:41pm

Beautiful set of bowls, Joe. They appear quite glossy. Not your usual matte combos over Strontium Crystal Magic. Could you talk about what's different with them from your other work?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service