Been looking for a c6 ox glaze as this one for a long time. Is green breaking dark green, verdigris, or oxidized copper glaze. Potter unknown.

Views: 211

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Daniel Ramos speak-spanish. on May 31, 2015 at 9:36am

Another idea to achieve the same effects seen on Ron Mello's vases, is trying an red iron red glaze perhaps the Recipe #451 from the Cooper book, or an an iron oxide engobe, with the # 200 or # 247 layered over it. Perhaps adding an extra opacifying in the covering glaze (to make it dryer or more mature ?)

Otra idea para lograr el efecto de las botellas de Ron Mello , es intentar poner el esmalte rojo de hierro  quizá el #451 o un engobe de hierro directo abajo    , y arriba poner el #200 o el #247 , quizá añadirle un opacificante extra y que el esmalte de arriba sea seco o poco maduro ,  cosa de  probarle 

Comment by Daniel Ramos speak-spanish. on May 31, 2015 at 8:40am

I'd like to figure out how Rom Mello applied this glaze from the Cooper book.


This really cool, I wonder how it was done?

El link te va mandar a una página de Facebook , pero en la barra de archivos del grupo se puede descargar el libro de Cooper en español , , en cuanto a el barniz que aplica el ceramista Ron Mello es este ,me gustaría aplicarlo , esta muy padre , me gustaría saber como se logró .

Comment by Daniel Ramos speak-spanish. on May 31, 2015 at 8:25am

Cone 7

Comment by Daniel Ramos speak-spanish. on May 31, 2015 at 8:23am

Comment by Daniel Ramos speak-spanish. on May 31, 2015 at 8:21am

Hello Norm Stuart, I also think the three color green, beige and red glaze is one glaze applied over another - a variation from the Emmanuel Cooper book, Recipe #200 on page 102.

Half of the Line-Blend tile has a white glaze which becomes more red.

A new test occurs to me, using the reverse, ir a white tin glaze with the glaze from Cooper Recipe #200 glaze layered over it.

I've seen a few pieces where the potter Ron Mello has used used two color glazes very effectively.

This is the link to the Cooper glazes in PDF format.

PDF file - Emmanuel Cooper Glaze Recipes in Spanish

Taken from this Facebook webpage.

http://www.facebook.com/groups/225665340931510/331596543671722/

I'd like try to find or develop the recipe, which I'll try firing in reduction in a gas kiln.

#200 Transparent Semi-Gloss Glaze  (Barnice Transparente Semipétreo)

60 Nepheline Syenite - (Sienita Nefelina)

10 Ferro Frit 3134 - (Frita de Bórax Standard Ferro 3134)

25 Calcium Carbonate - (Blanco de España)

5 Ball Clay - (Arcilla del Bollas)

Variation - Fires to a mottled green in oxidation and a mottled red-green in reduction.

1.5% Copper Oxide

Hola Norm Stuart, yo igual pienso que tu, Tres Colores verde, beige y rojo es superposición de esmalte, la ficha # 200-V corresponde ala Variación del libro de Cooper, La Mitad de la pastilla de prueba Tiene Un esmalte Blanco Que dio ONU rojo, se me ocurre en Una Nueva prueba · intentar al al revés, es Decir el esmalte Blanco con estaño abajo y el esmalte # 200- V superpuesto arriba. He visto Que El ceramista Ron Mello, Tiene Unas Aplicaciones de esmalte de dos colores muy bien logradas, está aquí el enlace de Cooper https://www.facebook.com/groups/225665340931510/331596543671722/, me gustaria Que intentaremos Encontrar o desarrollar La Receta, yo intentare encontrarla en horno de gas y Reducción   


Stars
Comment by Norm Stuart on May 30, 2015 at 11:16am

Please post the recipe, and I'll try it.

Por favor escribe la receta aqui, y lo intentaré.

Comment by Daniel Ramos speak-spanish. on May 30, 2015 at 8:07am
Hay un esmalte de Cooper que da beige , verde y rojo , es el #200 variación , anexo foto después

Stars
Comment by Norm Stuart on May 18, 2015 at 10:17am
I suspect this is one glaze layered over another.
.
Yo sospecho que esto es un esmalte en capas sobre otro.
Comment by Daniel Ramos speak-spanish. on May 17, 2015 at 6:55pm

Recipe Please .?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service