Comment by Joe Shaw on October 29, 2012 at 11:13am

Teresa,

You brought up a very interesting line of thought with your original question. Which leads me into thinking about what do we tell other potters and the knowledgeable collectors when we use glazes that have question marks about their usage and intended functionality? Are we implying that glazes which were questionable are now safe? Maybe, and that concerns me. My posting this image was merely as an example of Weathered Bronze. The message seems to be that I am endorsing Weathered Bronze for utilitarian ware. That's not the message I want to send at all because I don't without some caveats. The main thing to take away from this is to test under your own conditions. I don't use Weathered Bronze on food surfaces except for this platter. I use it on the exteriors of my mugs, glasses and bowls. I felt safe using it on a 17" platter. I think that might have been irresponsible on my part. Not because the ware was unsafe, I'm satisfied that in my case it is safe, but, because the image itself seems to imply my endorsement of the safety of this glaze and that concerns me. I think this would be a terrific topic for further dialogue.

Thanks again for the question, it is truly inspiring!

Joe Shaw


Stars
Comment by Teresa Wooden on October 29, 2012 at 9:24am

Thanks for the info, Joe.  It is a beautiful piece.  I will definitely have to experiment with the glaze.


Stars
Comment by Joe Shaw on October 29, 2012 at 9:18am
Carl,
Yes it was done with slip and thank you for your comment!

Stars
Comment by Joe Shaw on October 29, 2012 at 9:17am
Teresa,

There can be pin-hole issues when the glaze is too thick. I fire to a hard cone 6. I have tested using lemon slices and vinegar several times and have observed no leaching. It also doesn't "metal mark" either. The concerns I've read are more about hygiene due to pin-holing than leaching with this glaze when fired to a cone 6 and higher. Each of us should be testing our glazes because our conditions can vary so much. Matte surfaces are questionable in regards to food. Some mattes are under-fired and matte surfaces can present hygiene issues. I wouldn't recommend this glaze for food surfaces until you've done the testing under your own conditions.

Stars
Comment by Carl Ray Crutchfield on October 27, 2012 at 5:53am

beautiful piece, texture band adds much interest.  was it done with slip?


Stars
Comment by Teresa Wooden on October 25, 2012 at 2:54pm
Joe, can this be used on food surfaces? I use the CC Strontium matte only on sculptural pieces.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service