This is culmination of 3 glazes overlapped that I have been working on. A dolomite matte that is white, a milky clearish white, and a titanium white. Also a tad of fake ash sprayed lightly over it to give it the green hues on the right.

I am really happy with this and I think I could take it further. It has beautiful tones of brown and I loooove the way the rim breaks and the color that shows through. It is really spot on to what I have been trying to achieve. Unfortunately the black clay I have been working with doesn't have the same effect. Sort of a sad moment that I am probably going to give up on the black clay, so far I haven't had any luck in creating the tones I am looking for. This pot basically satisfies all my requirements.

Natural spots from the clay body, beautiful tones of brown, green, grey and white, and interesting surfaces.

Is it time to settle down and explore this? Can I commit. Ahhh

Views: 103

Albums: Stoneware

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Joseph Fireborn on June 11, 2017 at 12:45pm

carl thanks, the way you described it is very nice.


Stars
Comment by Carl Ray Crutchfield on June 11, 2017 at 11:10am

a very natural elegance fitting of the form, well done 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service