Views: 232

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Tracy Minarik on December 22, 2011 at 10:38pm

Just watch these glazes for running..

Especially the ash glazes.  Keep them towards the top till you figure them out more.

Also, Stronium Crystal Magic Cool is a runner also if not thinned right.

I've lost  plenty of pieces trying out these new glazes.
Try small test pots first.  Good luck! 


Stars
Comment by Tracy Minarik on December 21, 2011 at 7:31pm

It's all about the heat, the slow cool and the application..
What I did is make a large cylinder, overed it in SH Ston. Crystal Magic warm, devided it with lines about 3 inches apart around the whole thing then tested different amounts on it. Fired it in a scutt for the recommended times.  I tend to get better results in a scut then in my cone art kiln. I don't know what the difference is, but the Scutt brings this effect out better...  Crap shot sometimes...


Stars
Comment by Tracy Minarik on December 13, 2011 at 11:12am

I believe this is the Copper Ash glaze, fired to Steven Hills firing schedule.  This is put on last, over the Crystal Magic warm, sprayed from underneath to rim as to not get inside the cup.  That might have something to do with it.  I get different outcomes from the two different kilns I use. One Scutt, which I think this one came out of and my Cone Art.  Supposedly the same temps, but they fire differently for some reason...
Not too much, but not to little either.. try some test pots with different amounts and different hold times..  SLow cool is the trick I think....  Good Luck ~

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service