CHS on outside and FB without iron on the inside.

Views: 147

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Randy McCall on November 23, 2011 at 12:37pm
I use nutmeg because the version I use looks like wood fire shino. It has to be put on thin. I either pour on a thin coat or use a small natural sponge and put on a thin coat. The color varies from brick ed to cream. Coat thickness is the key with nutmeg.

Stars
Comment by martha peddicord on November 23, 2011 at 9:58am

Thanks, Randy.  Wonder if the nutmeg uses the same?  My nutmeg isn't as beautiful as some pics I see on here.


Stars
Comment by Randy McCall on November 23, 2011 at 8:59am

In order for it to work right you have to have Special red iron oxide.  It is called Special Red nothing else will work.  I got mine from US Pigments.


Stars
Comment by martha peddicord on November 23, 2011 at 5:58am

I used Spanish red, what is the name of what I should use?

I have crocus martis, is that better?


Stars
Comment by Randy McCall on November 23, 2011 at 5:42am
Sorry not I may have failed to mention that you have to use special red iron oxide that is a pure form of Rio.

Stars
Comment by martha peddicord on November 23, 2011 at 4:33am

Randy, I have tested this glaze and can only get a dark muddy cordovan look, like old 50's penny loafers.  yuch!  I used a 500* drop from peak to 1800, then a 125 hour drop to 16oo* and a 30 min hold there, then off.  any suggestions, I would really like this sort of a red, no luck so far.


Stars
Comment by Randy McCall on November 4, 2011 at 12:55pm
Yes it is oxidation.  Usually do an hour hold about 1750F.  Easy glaze.  Probably do not have to do hold.  Layers great.

Stars
Comment by Kathy Ransom on November 4, 2011 at 9:03am
It's beautiful! Is this achieved in oxidation?

Stars
Comment by Randy McCall on November 4, 2011 at 6:32am
Should be CHT or C Harris Tem. the glaze you gave me.  Great glaze.  Best iron red I have ever used.  Gets great depth when layering.  Very smooth feeling.  One of my favorites now.  Probably one of the best iron reds that few people know about in pottery.  Never saw it until I got on your site and I have been doing pottery since 1976.  Thanks for it.
Comment by George Lewter on November 4, 2011 at 6:25am
What is CHS?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service