On B-mix 5. Hannah's Fake Ash at the top. Jen's Juicy Fruit on the bottom

Views: 111

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Jan Wallace on May 5, 2011 at 9:42pm

Thanks George. I will read that discussion and let everyone know how i go with my tests. 

Comment by George Lewter on May 5, 2011 at 6:37pm

Hi Jan,

B-Mix is simply a "White Stoneware", meaning mainly that it doesn't contain any ingredients with a lot of iron or other coloring oxides that would darken it. I would think you could get similar results with another white stoneware or with porcelain as your clay body. Check my discussion How to Down-Fire a Manual Kiln with a Dawson Kiln Sitter for information on defeating the shutoff feature of a kiln sitter, and doing a controlled cool down on a manual kiln. After you've digested that information, reply in that forum with any questions you may have.  Generally, you can heat up as fast as your kiln will heat, but doing a soak at the maximum temperature of 30-60 minutes, and slowly cooling the kiln to about 1500 degrees Fahrenheit will markedly improve matte and semi-matte glazes, and allow more mixing of layered glossy glazes. 

Welcome to our network!


Stars
Comment by Jan Wallace on May 5, 2011 at 5:28pm
Hi George. As i from Australia, i have not heard of B-mix 5. Is it a buff clay or white? I am going to test some of the glazes on this site soon (new member) and also would like to ask a technical question please. I have a small electric kiln (39 x 39 cm) with a manual controller (10% to 100% energy regulator) and an auto shut off at set temp. What would you suggest for me with respect to the way i turn up kiln in order to gain the best results in my kiln? I have been reading a few things that suggest firing schedules to help those with controllers, so hence my question as this is very differant for me with a manual kiln. I would really appreciate your advice. Thanks.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service