SCM for cool colors under Opaque Blue Matt with a blue ash rim

Views: 159

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Michele Hartung on July 10, 2010 at 7:34am
Anthony, I am using the following schedule: 300 to 1600, 100 to 2232, hold one hour, then drop 300 to 1700, then turn off. This just gets me to a ^8. Here is the Blue Matt recipe:

Opaque Blue Matt w Strontium ^10
Strontium Carb 31.9
Nepheline Syenite 53.1
Tenn Ball Clay 6.7
Silica 8.3

Add:
Copper Carb 4
Bentonite 1

I am spraying fairly thin, however, I have not taken a measurement so cannot quantify that. The Blue Ash is Hannah's from Steven Hill's recipes. This pot also has an awesome interior that works well in electric. It is Penland Red-Orange applied very thickly. My next experiment is to see if I can get it to work on the outside as well as it works on the inside. Spraying the Penland does not allow for a thick enough coating and it turns a flat looking brown. Oh, by the way on this Opaque Blue, it runs like crazy so leave it light at the base and if you dip the pot, just dip the upper 1/2 or so. It's a very pretty glaze by itself, even without the SCM under it.
Comment by Anthony Andersen on July 9, 2010 at 11:14pm
I would love the recipe for both, but especially the blue matt as I have a couple pretty good recipes for fake blue ash (Hannah's and Steven Hill). Looks like the matt glaze is sprayed fairly thin - maybe 1 to 1.5 mm. Does that sound about right? Also, are you doing a slow cool down? My SCM schedule is currently a cone 8+ with peak temp of 2220 and an hour hold, then 150/hr down to 1700. I'm pretty sure my thermocouple is a little off so it's probably more like a peak of 2250 or a little higher.
Comment by Michele Hartung on July 9, 2010 at 3:31pm
Thanks very much! This is an opaque blue matt glaze and blue ash on the rim. If you want any recipes, just let me know.
Comment by Anthony Andersen on July 7, 2010 at 11:34pm
Very nice. Definitely 5 stars. What's the glaze? Something over SCM white?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service