Comment by John Talbot on March 30, 2012 at 6:31pm

Ya, I got this glaze out of a pottery book that I was learning from.  I don't mind sharing it at all.  Here's the recipe from my GlazeChem database:

Rootbeer Brown
---------------

Range: Cone 6
Firing type: Oxidation
Glaze type: Mid-fire
Color: Dark Brown
Surface: Semi-gloss to Gloss
Transparency: Translucent
Flow: None
Durability: Good
Testing: Tested

Recipe:
Custer feldspar   30.30
Whiting             25.60
EPK                   7.60
Silica                36.50
--------            -----
                      100.00

Red iron oxide     11.70

 

Variations:
Replace Iron Oxide w/ 5% Copper Carbonate = Glossy Green

Notes:
Semi matt dark brown thin to glossy amber thick
Great stable glaze, prime glaze for dishware

Glossy White over Rootbeer Brown = Specked Yellowish Tan (resembles bamboo over
textured pottery)

Source: From the diy network book "Wheel-Thrown Pottery"
Date: 08/11/2007

Comment by P. Cooper on March 24, 2012 at 4:27am

What is the brown glaze on the bottom half of these?  I have a glaze similar to this that i make from local clay that's dug in Bethune, SC.  It takes a ton of work to get the trash and rocks and stuff out of the clay and get it sieved fine enough to use in a glaze.  If you have a recipe it would help me tremendously.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service