Comment by Michele Hartung on May 10, 2011 at 7:24am
Sterry, thank you for your advice!  I will google these things and start a new adventure!  That red knocks me over.
Comment by §terry fallon on May 8, 2011 at 10:12am

Ms. Michele

 

Thanks for commenting on my copper red. Reduction in electric kilns is more common than you think.

Yes like anything, there is a right way and a wrong way to do it, unfortunately if done the wrong way it will damage the kiln.

However done correctly no damage is done. In addition, with a kiln built to do Electric-Reduction, you get even longer element life than a standard kiln.

Google “Electric reduction kiln” or “reducing in an electric kiln” or “Fallonator” there is lots of reading and research that has been done in the last ten years.

 

§terry              


Stars
Comment by Michele Hartung on May 3, 2011 at 2:48pm
Wow!  Congratulations on your electric/reduction kiln.  I didn't think this was possible.  Looks very complicated.  Thanks for sharing this with the community.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service