Views: 313

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Mark Hamilton on November 5, 2012 at 8:20pm

I found it here: http://www.greatclay.com/Merchant2/merchant.mvc?

You will have to go to stoneware glazes and page to it, its there in a long paginated list.

It's GL650 Blue Pearl.

 

I meant to ask Catherine what glaze is on the rim, inside as well...

 

 


Stars
Comment by Elaine Carroll on November 5, 2012 at 6:52pm
Mark, if you find the pearl blue, would you please post. I think the crackle is a Laguna glaze.
Comment by Mark Hamilton on November 5, 2012 at 6:38pm

Thanks. The depth is unreal - I will try.


Stars
Comment by Catherine Rehbein on November 5, 2012 at 4:43pm

Thanks Mark, Blue Pearl with Catalina Crackle....I spray on layers . Good Luck!

Below are  Links where I purchase my glazes

http://www.greatclay.com/Merchant2/merchant.mvc?Screen=CTGY&Cat...

http://www.minnesotaclayusa.com/glazes/glazes.html

Comment by Mark Hamilton on November 5, 2012 at 10:28am

WOW...this is a look I have been looking for in Cone 5/6. If you can, might you share the glaze names and method to obtain this look? It seems that you may have layered over the base glazes with a clear glaze? What were the base glazes, recall?


Stars
Comment by Catherine Rehbein on May 24, 2011 at 7:33pm

Thank you Lorraine! 

 

Comment by LORRAINE ADAMSON on May 23, 2011 at 7:10pm

I love your work.  

Amazing motion, amazing glaze treatment.


Stars
Comment by Catherine Rehbein on May 19, 2011 at 8:58am
Thanks again J....I had fun with these tea bowls. Stephen Hill chose 2 of these to be on display in the KC Teabowl National...What a surprise! Cant wait for the Opening!
Comment by J dubats on May 18, 2011 at 5:36pm

Another Wow.  Beautiful glaze color and movement.

 

Comment by Dale Duncan on April 13, 2011 at 5:27pm

I love the depth of the glaze on this piece.....Very Nice!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014