These Vases are wheel thrown and altered. The Base Gaze is Hamling's. The manual Kiln shutoff before I could start the slow cooling. I am really happy that this happens in my kiln without changing anything.

Views: 161

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Theresa Marie Shanks on July 1, 2013 at 8:27pm

Yes. I don't use pedestals.  I make catch basins.  I make a sawdust puck made from alumina Hydrate:epk:sawdust  1:1:.5 and brush coat it with alumina hydrate:epk 80:20.  I brush the 80:20 on the foot of the pot thick. I  shape a two inch high puck under the foot (the diameter as the base). Coat the puck and the base of the catch basin with the 80:20.  The Puck breaks loose of the basin and the puck can easily be removed from the pot.  I use a tile saw, if needed and I am going to buy a lap grinder to clean up the piece.


Stars
Comment by Norm Stuart on July 1, 2013 at 7:29pm

Theresa - Do you need to place a catch basins under under each piece with this zinc silicate glaze?

Comment by Amanda Sullivan on July 1, 2013 at 5:55pm

Thanks!

Comment by Theresa Marie Shanks on July 1, 2013 at 4:30pm

I put down the wrong Recipe.  

Silica is 15%

Zinc is 25%

3110 is 52%

The previous recipe minimized crazing but did not have as many crystal

I put Rutile in the base at 8%

Comment by Theresa Marie Shanks on June 30, 2013 at 7:49pm

Sure.

Frit 3110 52%

Zinc Oxide 24%

Silica 24%

Spanish Red -- Darker Glaze

Rutile 8%

Spanish Red Iron 2%

Manganese Dioxide 1%

Lighter Amber 

Manganese Dioxide 2%

Rutile 8%

Green

Copper Carbonate 3%

Rutile 8%

Blue

Nickle Oxide 3%

Comment by Amanda Sullivan on June 30, 2013 at 7:34pm

Are you willing to share the base glaze?? It is so beautiful!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service