Comment by §terry fallon on February 3, 2011 at 4:24am

Yes I use computer control over the reduction level. I use the same software to control the reduction level as the Bartlett controler uses to control the heating of the kiln.

 

For the element life, yes reduction reduces the element life.

My fix for this was, a new way of suppling the curent to inprove the element life three fold. My Kilns do more than 100 cone 10 firing to a set of elements.

I have had reportsd back as many as 300 firings at cone 10.

Google search “ Fallonator reduction” I am the first 19 results

§terry

Comment by Zoophagous on February 2, 2011 at 7:41pm

Wow, I am amazed. 

 

More questions cuz I am a glaze geek.

 

My assumption is that your equipment give you a very tight control over the time and amount reduction, is that a correct assumption?

 

Also, my understanding is that reduction shortens the life of electric kiln elements. Have you found that to be the case?

 

Thanks for sharing your work. It's potters like you who make the rest of us better.

Comment by §terry fallon on February 1, 2011 at 4:59pm

 

This copper red is “Rhodes 30” a well published stoneware copper red glaze.

No locale reducing agent. Propane is the reduction agent, I can convert most electric kiln to do the same. The entire kiln is put into reduction by computer controlled.

Here is a link that will shed some light.

   http://s3.excoboard.com/crystal/64697/789956

 

Google search Fallonator or Fallonator reduction

Wait and see what happens after the 2011 NCECA conference in Tampa.

 

§terry

Comment by Zoophagous on January 30, 2011 at 10:09pm

I have to ask - how are you getting such great copper reds in an electric kiln? Are you using a reducing agent in the glaze or are you reducing the entire kiln?

And you should be proud - your copper reds are beautiful.

Comment by §terry fallon on January 23, 2011 at 6:30pm
Comment by Zoophagous on January 23, 2011 at 5:36pm
Amazing. Nothing compares to a good copper red.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service