Potters & Sculptors - Making Rock from Mud
Black slip with June Perry's Purple and Floating Blue over. can't wait to try this out on a bowl.
Tags:
Albums: Cone 6 test pieces
Comment
Hi George,
Found the recipe on my e-reader, it's quite different. Here goes.
21 Gerstley Borate
16 Neph Syen
11 China Clay
32 Silica
20 Whiting
5 Tin Oxide
0.15 Chromium Oxide (had to guess this tiny amount)
*Nice purples by adding small amounts of cobalt
Good luck, Love to see your results.
Cheers,
Jenny
II'm not sure, will have to wait til I get home to check. On the high seas at the moment cruising around New Zealand.
Is this the recipe for the purple you used? On June Perry's website it is listed as
Clayart Purple glaze #6472
37 Custer Feldspar
12 Gerstley Borate
6 Dolomite
14 Talc
3 Zinc Oxide
5 EPK
23 Silica
Total 100
ADD: Cobalt Carbonate 3, Bentonite 2
+1.... Looks like this has a lot of potential..
Very nice. I would like to see what it will do breaking on high spots.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics