The same crystalline recipe & batch was applied to three different porcelain clay bodies with various levels of oxides. The resulting changes in glaze appearance was produced by the clay, not the glaze.

Views: 133

Albums: Clay Tests

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Tom Anderson on September 1, 2017 at 4:17pm
Josi:
The one on the left has the most oxide additions. It turned the usual hi- gloss/ hi-opacity of crystalline to matte. The one in the middle, I was going for translucency: but not thin enough. Always thought crystals would pop more on highly translucent pieces.
Tom
Comment by josi rica on September 1, 2017 at 11:40am

Very interesting to see the various colors just on simple different clay

Is it the one of the center which contains most oxide?


Stars
Comment by Tom Anderson on August 29, 2017 at 8:45pm
Norm: just realized I misread your post. (Reaches for glasses.)
I have a PP VPM 20 I use to mix colored porcelains because it is the easiest and quickest to clean. Will have a Bailey VPX 125 in here shortly for production (400lbs) an hour mix rate.) looking at some open mill augers that mix 1000-3000 lbs at a time. See where it hoes and how it grows.

Tom

Stars
Comment by Tom Anderson on August 29, 2017 at 6:34pm
Forgot to mention: my speciality clay line has been picked up by a couple of local suppliers. Sometime in October cone 04 porcelain and colored porcelain will come out. Then cone 6 colored and speciality porcelain in November: if my schedule holds.

Stars
Comment by Tom Anderson on August 29, 2017 at 6:31pm
Norm:
No, never worked for any clay companies. Been studying clay formulation and chemistry for years. Have several formulation articles coming out in Ceramics Monthly over the next several months. Studied with Ron Roy on and off: the man who taught Tony in part. Been working on clay formula limits, formulation criteria, and SAS theorem.
I have seen Tony's 03 formula: he is a big fan of V- Gum,whereas I am not. I talk to Tony on rare occasions via email.
Tom

Stars
Comment by Norm Stuart on August 29, 2017 at 11:53am

What do you use to mix clay?

The only time I've mixed clay, Tony Hansen's Cone 03 porcelain, I added enough water so I could use a cake mixer, then hung it up in cloth to dewater.


Stars
Comment by Tom Anderson on August 28, 2017 at 9:09am

I mixed clay all weekend: all cone six except for a special order of cone 11 porcelain.

100 lbs of standard porcelain, 100 lbs of 0% absorption stoneware, 100 lbs of Redstone, and a two different colored porcelains. This coming week I am going to make some clay for me... special crystalline porcelain.

Tom

Comment by Joseph Fireborn on August 28, 2017 at 8:10am

They are all very nice!


Stars
Comment by Tom Anderson on August 23, 2017 at 4:56pm
Joseph:
The one on the left ended up being matte, which I found unique for crystalline. The one on the right is common, so not much surprise there. The one in the middle was the one I was hanging my hopes on: translucent body. Did not get it thin enough to really produce that effect, it has some degree, but very little.
Tom
Comment by Joseph Fireborn on August 23, 2017 at 9:32am

Which was your favorite? 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service