Tangerine Glaze Crystals in a Yellow Mason Stain glaze. Porcelain over a paper-clay base.

Last year we searched for "Glaze Crystals" for a granite look or other crystal glazes and found the industry supplier in Maryland. They melt into larger patterns at ^6 shown here, or can be used at ^06.

http://www.rabcospecks.com/home.cfm

To use their "online store" you need to request a catalog. We ordered mostly larger mesh and crush them if people want smaller crystals. You can combine them to make any of the looks shown in these prepared Mayco Jungle Gem glazes.

http://www.maycocolors.com/index.php?option=com_virtuemart&category_id=69&page=shop.browse&Itemid=4

Here's the price per pound we paid, comparable to Mason Colors. Needless to say, their range of stock is larger than what we purchased:

$13.85 _ FLG-460 _ Dark Golden Rod Crystals 6/16/Mesh (8 oz)
$14.08 _ FLG-470 _ White Crystals 6/10 Mesh (8 oz)
$14.68 _ FLG-489 _ Moss Green Crystals 6/20 Mesh (8 oz)
$14.08 _ FLG-491 _ Chartreuse Crystals 6/20 Mesh (8 oz)
$16.73 _ FLG-495 _ Yellow Crystals 6/20 Mesh (8 oz)
$15.28 _ FLG-514 _ Burnt Orange Crystals 6/20 Mesh (8 oz)
$19.38 _ FLG-541 _ Red Crystals 6/16 Mesh (8 oz)
$15.05 _ FLG-547 _ Blue Crystals 6/20 Mesh (8 oz)
$14.85 _ FLG-555 _ Tangerine Crystals 6/20 Mesh
$14.08 _ FLG-556 _ Reactive Metallic Crystals 6/16 Mesh (8 oz)

Views: 5901

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on April 9, 2013 at 1:06pm

This is a typical look at ^06 in a white base glaze.

FLG-464 Blue Crystals 6/16 Mesh

FLG-541 Red Crystals 6/16 Mesh

This Mayco "Wildfire" ^06 prepared glaze uses larger mesh yellow "reactive" crystals with smaller mesh brown crystals. Rabco uses the word "reactive" for crystals which bloom in "unpredictable ways".

From their website:

RABCO, Inc. has been supplying Ceramic Glaze Crystals for use in ceramic coatings since 1979. Our customer list includes virtually all domestic manufacturers of glazed wall and floor tile, commercial dinnerware and cookware, prepared hobby glazes, lamp bases and artware, structural clay products, specialty porcelain and sanitary ware. In addition to the conventional “gold dust” and “salt & pepper” effects, Glaze Crystals can be used in many other ways to provide your products with new and different looks.

Our regular Glaze Crystals offer another design tool to enhance the "flat" look of many ceramic coatings. These materials can introduce complimentary or contrasting colors to the background color.
 
Combining several colors and sizes can result in the ever-popular "Granite" look. Using only one color in a disco-applied granite glaze can shift the overall color effect without another glaze application.
 
RABCO Glaze Crystals can simulate iron spots on brick and quarry tile surfaces and can be used to produce the ever popular "enamel ware" coatings on white ware bodies. Also, we offer "reactive" Glaze Crystals, the use of which can produce unusual and often unpredictable results in certain glaze compositions.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service