A slab of stoneware clay was enhanced with clay chalks before being made into this lidded coffer. After the bisque, I wax resist painted circles on the chalked surface, then glazed around the circles. Leather cords and ceramic tassels form the belted accent.

Views: 105

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Barbara Hanselman on April 7, 2019 at 10:14am

The large leaf plate made by one of my students who is very adept at making clay chalks, is pictured below.

Comment by Barbara Hanselman on April 7, 2019 at 10:13am

Comment by Barbara Hanselman on April 7, 2019 at 10:11am

Clay chalks are something you can make then use like pastels on the bisqued clay surface or use sifted through a fine mesh sieve on to the greenware surface. By rubbing the chalk across the mesh, it is deposited on the greenware surface in a fine powder (wear a mask!) and can almost resemble airbrushing.

Ceramic Pencil or Chalk Slip Recipe

 

White firing ball clay

50%

 

Potash feldspar

25

 

Silica

25

 

 

100%

Add:

Macaloid (or 5% bentonite)

3%

 

Colorant (maximum)

15%

 

 

http://ceramicartsdaily.org/ceramic-supplies/underglaze-ceramic-supplies-2/drawn-to-surface-how-to-make-and-use-underglaze-pencils-crayons-pens-and-trailers/

 

 

https://www.youtube.com/watch?v=jm7I0_P0jhc

https://www.youtube.com/watch?v=HcsMRap70lE

 


Stars
Comment by Norm Stuart on January 25, 2019 at 9:28pm

What are clay chalks?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service