Opulence glazes:
Autumn Frost over Black
Clay is Standard 378

Views: 268

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Sharon Ivy on February 18, 2012 at 4:32am

Craig, we have tried other colors, but no satisfactory results yet.  I really wanted it to work over my MC6G Licorice since it's a much smoother, nicer black, but the crackles were very wimpy over the Licorice.

When we mixed a new batch of Autumn Frost not long ago, we found it didn't break up as well as the old batch had and it was settling out really quickly.  After adding some muriatic acid, though, it went back to giving us these results.  You can tell it will work if the Autumn Frost begins to crackle and buckle up a bit while drying.  Otherwise, you get just a smooth golden glaze during firing. Has been fun to play with and my husband continues to experiment with it.

Comment by Craig Roth on February 18, 2012 at 4:21am

Super interesting!  Have you tried other colors?

Thanks for sharing.

Comment by Sharon Ivy on December 23, 2011 at 7:26pm
I think the Opulence glazes would work fine with the way you normally fire. I find them not to be too finicky. I have only tried this combo with the Std 378 clay. I'd be interested to know how it works if you do test it and use a different body. I do love the results I get, in general, with a slow cool, but who's to say yours wouldn't be perfectly satisfactory, too!
Comment by Sharon Ivy on December 10, 2011 at 2:33pm

Hi Cathy!  So glad you're giving this pottery thing a go.  Always good to have new potters interested in the craft.  I, too, am relatively new to glaze development and do have a couple I'm experimenting with, but the 2 glazes on this mug are straight commercially available glazes.  They are Opulence brand and I buy mine from Mid-South Ceramics in Nashville TN.  You can order online.  The Black is #127 and shows under the Glossy section.  Autumn Frost is #601 and is under the Reduction Look section.  I dip the entire cup in Black, let it dry just a bit, then dip just the rim area in the Autumn Frost.  That's it! 

I bisque to cone 04, then glaze fire using the schedule in Mastering Cone 6 Glazes.  If you don't have this book, I highly recommend you get it.  They have their firing schedule on their site here http://www.masteringglazes.com/Pages/faqframe.html.

Feel free to contact me with more questions.  I'm a former art teacher and love sharing anything I can to assist other artists.  Good luck!

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service