Red and white terrasig. Chicken feather and sugar applied on taking out of raku kiln.

Views: 111

Albums: RAKU

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Donna Ferrara on April 25, 2012 at 3:53pm

thanks Jan.  In the past I haven't had any problem with the horse hair, but I was using the wrong feathers...just trying anything I found on the ground....I guess I have to find me some chickens!  I really like the effect with the sugar.  so 900C is around 1500-1600F?  I think I fire a little cooler, not by much.  I had trouble with cracking, but I heat up a piece of broken shelf in the kiln too, and then put the pots on that.  It seemed to help some.


Stars
Comment by Jan Wallace on April 25, 2012 at 3:40pm

Hi Donna, I have personally found that with horse hair and feathers, the pots cannot be too hot when you take them from the kiln as the feathers and horsehair just repel or bounce off. It's happened to me when I have tried at about 950deg c. The pots are also more likely to crack at this temp, especially since for these little pieces I used white earthenware, coated with a terrasigillata as a pose to a grogged clay for raku. I think the best temp is from about 800 - 900deg c. Soft feathers are also best (this is a bantam feather from my little bantam chicken) and if they have a natural curve I take advantage of this and hold the curved side against the pot. I have also used sugar on this pot by sprinkling over the pot whilst hot which creates the little round halo's/dots when it burns onto the pot.


Stars
Comment by Donna Ferrara on April 25, 2012 at 4:32am

really lovely! - i've never had any luck with feathers, how do you do that?  does it need the sugar for the image?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service