Views: 169

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Jeff Poulter on April 20, 2012 at 3:43pm
I think you could spray the blue-amber and then spray a light coat of the white liner and then sponge on some more white liner. I think it would work. But you know how they say to test, test, test!

Stars
Comment by Randy McCall on April 20, 2012 at 2:57pm

Jeff one thing that I failed to mention was the fact that I sponge on an irregular

top coat with an small natural sea sponge.


Stars
Comment by Jeff Poulter on April 18, 2012 at 11:59am

Creamy White Liner

G-200     20.0

FF 3134  20.0

Wollastonite  15.0

EPK   20.0

Talc  6.0

Silica   19.0

Add Tin Oxide   4.0

Amber

Custer   30.27

Whiting  25.65

Silica  36.53

EPK  7.55

Add RIO  11.66

  On this one I did away with the RIO & added Cobalt Carb.  W/O my notes I would say about 1-2 %.   I sprayed on the Blue/Amber first & then sprayed on the Creamy white Liner.


Stars
Comment by Tori Sheppeard on April 18, 2012 at 11:38am

Yes, I would love try the recipe as well.  Thanks


Stars
Comment by Randy McCall on April 18, 2012 at 11:28am

We would like to try the recipes if you don't mind.


Stars
Comment by Jeff Poulter on April 18, 2012 at 10:27am

Hi Randy & Tori,

    Here are a couple of the pots that I used the combo on.  I wanted more white & more intermixing like Randy is getting.  Also the aventurine that I put on the rims didn't do what I wanted either.  If you want I can post the recipes.


Stars
Comment by Randy McCall on April 17, 2012 at 6:13pm

Thanks.  I am always searching for those spectacular patterned glazes.  Great.  Always look forward

to experimenting and trying something different.


Stars
Comment by Jeff Poulter on April 17, 2012 at 5:16pm
Fetish Ghost has a glaze combo that he calls Bone Marrow that is his White Liner over his Amber. I have been working on modifying the Amber to blue and then put the white liner over that. It isn't quite where I want it, but it is progressing. I will try and find a pic. Also I could find the recipes of you guys want to fiddle with it, too.

Stars
Comment by Randy McCall on April 17, 2012 at 3:46pm

Tori

I have never been able to produce this effect in oxidation with one glaze.  I fired Floating Blue without iron oxide to C6 then applied a heavy sponged coat of FB base with rutile, tin,  and copper carb then fired again to C6.  Quick up and down.  No holds.  If you do just one firing you will get the varigation you see, but probably will turn an olive green pattern glaze.  You will just have to try it and see.  I am going to try some experiments to see if I can get it in one firing.  I have been trying to find this glaze effect in ox for 30 years and just came across it trying to corrects some mistakes.


Stars
Comment by Tori Sheppeard on April 17, 2012 at 1:36pm

I love that glaze.  What glaze are you using on this piece?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service