Dry assembled greenware extrusions dipped in 85% phosphoric acid converting much of the kaolin to aluminum phosphate and silica and converting any carbonates present into gas bubbles within the greenware.

After bisque firing it was dipped in a solution of Pearl Ash and Boric Acid to create a K Metaphosphate and KBO2.KPO3 Eutectic. (see Insight Live for this Eutectic)

When dry I placed the sculpture inside a black plastic garbage bag and soaked it well with Bailey Shino (see recipe in the Insight-Live database) and fired to Cone 7.

Cone 6 porcelain (Laguna WC-861).

Phosphoric acid, used to flavor Coca-Cola with a tart lemony taste, is a fairly weak acid even concentrated at 85% with the consistency of honey and a high affinity for the 14% water it's mixed with. As a consequence after dipping the greenware in the syrupy acid, the clay retains its dry appearance for 5 minutes or so until the foaming reaction begins. I didn't wear gloves, but it's a good idea.

85% Phosphoric Acid mixed with Wollastonite is a nearly ideal repair putty for refractory kiln brick - also known as Calcium Phosphate Cement.

Powdered 100% phosphoric acid is used as a very powerful dehydrator as it's binding affinity with water is far stronger than almost any other material.

Views: 103

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service