Comment by Don Olliff on January 9, 2012 at 8:22am

This piece is made with Nara ^5-6 porcelain bisque fired to 07 and then sprayed with two layers. Spearmint over whole piece and Variegated Blue over the top and shoulder. The blue on the sides is a reflection from the San Diego sky. :-) The inside was done with Variegated Blue.

Comment by eleanor akowitz on January 9, 2012 at 7:48am

don- love this pot! could you post the glazes that were used. also would be interested if the glazes were sprayed or dipped or brushed.  i wish you could do this for all your pots. all of them are lovely, but if you posted the info with each pot we would not have to ask additional questions.  it really is nice to have all the info together with the photo.

thanks

eleanor

Comment by Don Olliff on January 9, 2012 at 6:48am

Thank you Jette!

Comment by Jette Nielsen on January 9, 2012 at 5:43am

Almost look like carbon trapping, very pretty

Comment by cp dunbar on November 2, 2011 at 8:20pm
the glaze is rapturous, of course , but the feet, though subtle, increase the value of this pot greatly.
Comment by Jan Wallace on August 5, 2011 at 2:44am
This is so pretty. Can you please share what glaze this is?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service